Comparision of Properties |
FRP |
PVX |
Steel |
Aluminium |
|---|---|---|---|---|
Dendity t/m3 |
1,6-2,0 |
1,4 |
7,8 |
2,7 |
Tensile strength MPa/m2 |
410-1180 |
41-48 |
410-480 |
80-430 |
Flexural strength MPa/m2 |
690-1240 |
30-110 |
400 |
275 |
Tensile modulus GPa |
21-41 |
2,8 |
210 |
70 |
Coeficient of linear expansion 10-6 C-1 |
5-14 |
54-75 |
11-14 |
2,2-2,3 |
Thermal conductivity W/m2 |
0,3-0,35 |
0,3 |
46 |
140-190 |




































| a, mm | b, mm | c, mm |
| 40 | 30 | 4 |
| 50 | 30 | 4 |
| 60 | 30 | 4 |
| 75 | 30 | 4 |
| 80 | 30 | 4 |
| 100 | 30 | 4 |
| 120 | 30 | 4 |
| 125 | 30 | 4 |
| 140 | 30 | 4 |
| 150 | 30 | 4 |
| 200 | 30 | 4 |
| 250 | 30 | 4 |


| A, mm | B, mm | C, mm | ||||||
| 50 | 10 | 250 | ||||||
| 50 | 10 | 300 | ||||||
| 50 | 10 | 350 | ||||||
| 50 | 10 | 400 | ||||||
| 50 | 10 | 450 | ||||||
| 50 | 10 | 500 |


| a, mm | b, mm | c, mm | ||||||
| 70 | 50 | 4 |


| A, mm | B, mm | C, mm | ||||||
| 200 | 70 | 8 | ||||||
| 250 | 70 | 8 | ||||||
| 300 | 70 | 8 |